Humping Welding Phenomena Produced by Pulsed High Current GTAW of Steel 100Ar
Welding discontinuities
High speed video of high current GTAW that produces a local gouging condition. This can occur in high productivity GTAW, and produces periodically displaced weld material adjacent to the bead, otherwise known as humping.
Back to top